TECHNET Archives

September 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Mon, 27 Sep 2004 14:40:21 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Black, Paul" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Black, Paul" <[log in to unmask]>
Parts/Attachments:
text/plain (97 lines)
Joe,

I would agree with George on both counts. In any case, I wouldn't choose HASL. It doesn't deposit evenly. In the case of your fine pitch and small components, you could end up with reliability issues.

Thank you, 
Paul Black 
Manufacturing Engineer 
Kronos 
E-mail: [log in to unmask] 
Voice: (978) 947-1520 
Fax: (978) 244-0568 
www.kronos.com 
Improving the Performance of People and Business(tm) 



-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Wenger, George M.
Sent: Monday, September 27, 2004 1:21 PM
To: [log in to unmask]
Subject: Re: [TN] ENIG vs. HASL plating with 0.5 mm pitch QFN components


Joe,

Were you asked to recommend the type of pwb plating that is best for your simple board or were you only given two choices to pick from?  If I had to pick from the two choices I'd pick ENIG.  If I had to make a recommendation I wouldn't recommend either.  My preference would be immersion silver.

Regards,
George

George M. Wenger (908)-546-4531 
Reliability / FMA Engineer
Base Station and Subsystems Group
Andrew Corporation,  40 Technology Drive, Warren, NJ 07059
[log in to unmask]



-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Macko, Joe @ IEC
Sent: Monday, September 27, 2004 1:08 PM
To: [log in to unmask]
Subject: [TN] ENIG vs. HASL plating with 0.5 mm pitch QFN components


Fellow techs,

I have been asked to recommend the type of pwb plating that is best for a
simple board with only a few components.  The finest pitch component is a
QFN, 64 pads, 0.5 mm pitch.  There are some 0402 resistors and capacitors as
well.

My 2 choices are HASL or ENIG.  Would someone please comment on which is
best for 0402  and 0.5 mm QFN type components.

Thanks in advance.
joe

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

------------------------------------------------------------------------------------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.  
If you have received it in error, please notify the sender
immediately and delete the original.  Any unauthorized use of
this email is prohibited.
------------------------------------------------------------------------------------------------
[mf2]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2