TECHNET Archives

February 2012

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 17 Feb 2012 22:53:26 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Message-ID:
Subject:
From:
Joyce Koo <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
<52135AE4151D8343B16989B2BFBED7DA1D52658221@pfc-dc01>
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
Parts/Attachments:
text/plain (23 lines)
Laser scan ?
--------------------------
Sent using BlackBerry


----- Original Message -----
From: Steven Kelly [mailto:[log in to unmask]]
Sent: Friday, February 17, 2012 05:13 PM
To: [log in to unmask] <[log in to unmask]>
Subject: [TN] Late Friday Question

Hi All,
Do you think it is possible to do Moire Inferometry on the ZIF end of a flex circuit to measure the co-planarity of a HASL finish across the width of the ZIF as well as along the finger length? My concern among other things is how to keep the ZIF end flat while doing the measurement?
Thanks. Steve Kelly

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2