TECHNET Archives

September 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Lyon Yuan <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 4 Sep 2013 19:03:34 +0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (1 lines)
hi ben,

it is pad missing from bga
在2013/09/04, "Gumpert, Ben" <[log in to unmask]> 写道:
Lyon, By 'pad drop' do you mean lifted pads? (Pads stayed with the BGA?) Usually this means that there wasn't enough heat - that the solder was not melted in all locations. Ben -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Lyon Yuan Sent: Wednesday, September 04, 2013 6:40 AM To: [log in to unmask] Subject: EXTERNAL: [TN] BGA pad drop guys,we found a few BGA pad drop after removed from pcba boards.what is reason to cause the issue ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2