These type of shorts are mainly due to either improper
inner layer etching (clearing the copper from inner layer
clearance pads) or drill to inner layer mis-registration.
If many shorts are detrected on the same board, that
typically points to mis-registration. Hope this helps.

Eddie Rocha
Director of Engineering
(408) 978-8992 x282

Hi Technetters,

Can any of the technical Gurus from the PWB Fab or related
industry
enlighten how & why the inner-layer power/GND shorts occur
& how they can
be detected after the boards have been laminated. Of course
I do understand
that when you are building boards with very tight
tolerances, fine lines
thin cores the probability of these type of shorts
occurring is quite high.
However we have days when we have zero GND shorts & days
with upto 5%. We
have looked into all potential problems, but maybe we are
still missing out
something, so if someone out there can enlighten me it will
be very much
appreciated.

Thanks,
Krishnan.C
Sanmina-SCI

---------------------------------------------------
Technet Mail List provided as a service by IPC using
LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with
following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send
e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at
[log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2