     Contact Steve Beigle @Alpha Metals
     714.757.0111


______________________________ Reply Separator _________________________________
Subject: Re: Assembly: Silver PWA Finishes
Author:  [log in to unmask] at corp
Date:    7/11/96 2:32 PM


     There have been some discussions right here in the last week, titled 
     "Silver Plating over Copper"
     
     
     MB
______________________________ Reply Separator _________________________________
Subject: Assembly: Silver PWA Finishes
Author:  [log in to unmask] at SMTPLINK-HADCO 
Date:    7/9/96 02:59 PM
     
     
     Good Morning Technet!
     
     Just a general question - I am in the process of looking at 
     alternative surface finishes for printed wiring assemblies. I have 
     done the usual paper searches and have some baseline testing 
     progressing on palladium,silver, and immersion gold finishes. Has 
     anyone had good success with implementing a silver finish on PWAs in 
     the production environment? Any migration problems? Any solder joint 
     reliability problems?
     
     
     Dave Hillman
     Rockwell Collins
     [log in to unmask]
     
The mail list is provided by IPC using SmartList v3.05
To unsubscribe from this list at any time, send a message to: 
[log in to unmask] with <subject: unsubscribe> and no text. 
     
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To unsubscribe from this list at any time, send a message to:           * 
* [log in to unmask] with <subject: unsubscribe> and no text.        * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2