TECHNET Archives

March 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Ellsworth D. Berkowitz" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Ellsworth D. Berkowitz
Date:
Wed, 30 Mar 2005 16:08:17 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (289 lines)
>-----------------------------------------------------

I encountered a similar problem with a previous employer some years ago.

I procured some basic paint stripper from a major home repair retailer.  It
was the the "super thick" formulation.  I masked-off the to-be-stripped area
 with kapton tape (masked slightly undersized, as I recall, as some stripper
will inevitably sneak under the tape).  Applied the stripper sparingly with
a swab or other suitable applicator.  Observed the LPI, and when it began to
bubble/blister, easily removed the softened mask with a swab.  I remember
approx. 5-10 minutes for the stripper to do its job.  Stubborn bits may
require a poke with an orange stick, toothpick, etc.  Really stubborn bits,
or especially thick coatings, may require a second stripper application.
Generously cleaned & rinsed the area with IPA and DI.  Dried & tinned the
exposed copper plane.

Of course, this was all done in a properly ventilated area, wearing all
pertinent safety gear.  This worked quite well, as an engineering-controlled
process.

Hope this helps. => ells

>---------------------------------------------------
On Wed, 30 Mar 2005 13:42:27 -0600, Genny Gibbard <[log in to unmask]>
wrote:

>Another thing along the same lines - but doesn't do it as neat as what you
>did, Steve, is apply some solder to some solder wick and rub the solderwick
>back and forth on the board, using a soldering iron - removes mask and tins
>the underlying copper in one step...
>
>Similar to Ramon's suggestion - heat is applied, and the abrasiveness of the
>wick scrapes the soldermask off, but might be slightly less abusive to the
>iron tip than the suggestion below.
>
>-----Original Message-----
>From: Dehoyos, Ramon [mailto:[log in to unmask]]
>Sent: 30-Mar-05 1:17 PM
>To: [log in to unmask]
>Subject: Re: [TN] Selective LPI soldermask removal...
>
>
>        Hi Steve:
>                        I have used on green LPI, a heat gun and a somewhat
>sharp wide solder iron tip. Move the heat around the area and scrap the
>masking with the tip. It comes off very fast.
>        Regards,
>        Ramon
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]]On Behalf Of Stephen Gregory
>Sent: Wednesday, March 30, 2005 1:59 PM
>To: [log in to unmask]
>Subject: Re: [TN] Selective LPI soldermask removal...
>
>
>I  messed up the URL in my email, some may have figured that
>out. But it's: http://www.stevezeva.homestead.com
>
>
>Kind regards,
>
>-Steve Gregory-
>Senior Process Engineer
>LaBarge Incorporated
>Tulsa, Oklahoma
>(918) 459-2285
>(918) 459-2350 FAX
>
>
>|---------+----------------------------->
>|         |           Jeffrey Bush      |
>|         |           <Jeffrey.Bush@VTCI|
>|         |           RCUITS.COM>       |
>|         |           Sent by: TechNet  |
>|         |           <[log in to unmask]> |
>|         |                             |
>|         |                             |
>|         |           03/30/2005 12:39  |
>|         |           PM                |
>|         |           Please respond to |
>|         |           TechNet E-Mail    |
>|         |           Forum; Please     |
>|         |           respond to Jeffrey|
>|         |           Bush              |
>|         |                             |
>|---------+----------------------------->
>
>>---------------------------------------------------------------------------
>-----------------------------------|
>  |
>|
>  |       To:       [log in to unmask]
>|
>  |       cc:
>|
>  |       Subject:  Re: [TN] Selective LPI soldermask removal...
>|
>
>>---------------------------------------------------------------------------
>-----------------------------------|
>
>
>
>
>We could do this for you with laser.
>
>Jeffrey Bush
>Director, Quality Assurance and Technical Support
>
>VERMONT CIRCUITS INCORPORATED
>  76 Technology Drive - POB 1890
>    Brattleboro, Vermont 05302
>      Voice: 802.257.4571.21 Fax: 802.257.0011
>           http://www.vtcircuits.com
>
>
>-----Original Message-----
>From: Stephen Gregory [mailto:[log in to unmask]]
>Sent: Wednesday, March 30, 2005 12:25 PM
>To: [log in to unmask]
>Subject: [TN] Selective LPI soldermask removal...
>
>Happy "Hump-day"!
>
>I might have asked the list about this over a year ago, I can't
>remember.
>But I have this
>assembly that goes into a Radar system. There's a device on the assembly
>that has to
>be sitting over the metal of the top layer plane, with no solder mask on
>the board beneath
>the footprint of the device for it to work properly. Unfortunately, the
>solder mask file in the
>gerbers didn't reflect this. So at the time (over a year ago), I
>reworked
>the boards that we
>had to correct the problem...and let me tell you, it's a REAL PIA!
>
>Go to: http://www.stevzeva.homestead.com and look at "Mask Removal", and
>"After Tinning"
>to see what I'm trying to do.
>
>I did this over a year ago, and we got an order for these assemblies
>again...but the gerber never
>got corrected, and I get to do this again. WHOOPEE!
>
>I have to remove the solder mask beneath where the device is going to be
>installed, and then
>I solder coat the area to cover the exposed copper. I'm removing the
>solder
>mask very, very
>carefully with a Dremel and a very fine abrasive tip, and I'm using an
>exacto knife with various
>blades. This is all being done tediously under a microscope to prevent
>the
>copper from being
>removed from the plane. We have a micro-blaster here to remove conformal
>coating, but it can't
>get down to the bare copper. That's why I'm using the Dremel and exacto
>knife. This time when
>the board house did their micro-etch or pumice scrub just prior to
>applying
>the solder mask, they
>really did a good job! That mask is on there, and meant to stay put! I'm
>really having a hell of a
>time doing this on these latest fabs.
>
>Is there any other way to remove this coating in the area that I need
>to?
>I'm thinking maybe a
>laser. Does anybody know where I would go to get this done, and about
>what
>it would cost?
>There's only 5-boards that I need this done to, but it takes me a couple
>of
>hours with each board
>to complete the job.
>
>Kind regards,
>
>-Steve Gregory-
>Senior Process Engineer
>LaBarge Incorporated
>Tulsa, Oklahoma
>(918) 459-2285
>(918) 459-2350 FAX
>__________________________________________________________________
>This message may contain information that is privileged and confidential
>to
>LaBarge, Inc.  It is for use only by the individual or entity named
>above.
>If you are not the intended recipient, you may not copy, use or deliver
>this message to anyone.  In such event, you should destroy the message
>and
>kindly notify the sender by reply e-mail.
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text
>in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at:
>http://listserv.ipc.org/archives
>Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
>ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>
>
>
>__________________________________________________________________
>This message may contain information that is privileged and confidential to
>LaBarge, Inc.  It is for use only by the individual or entity named above.
>If you are not the intended recipient, you may not copy, use or deliver
>this message to anyone.  In such event, you should destroy the message and
>kindly notify the sender by reply e-mail.
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2