The suffix is the impurity level. You can find all of this documented in
J-STD-006.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of ekalgren
Sent: Friday, January 05, 2007 1:51 PM
To: [log in to unmask]
Subject: Re: [TN] Solder Designations
Does the A or B refer to the metal's position in the composition
formula?
Sn60Pb40 = Sn60A
Sn62Pb36Ag02 = Pb36B
Sn63Pb37 = Sn63A
Eric Kalgren
Electrical Engineer
Cobham Defense Electronic Systems
Continental Microwave Division
11 Continental Drive
Exeter, NH 03833 USA
Tel: 603-775-5200
Fax: 603-775-5201
E-mail:[log in to unmask]
Website: http://www.cobhamdes.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gregg A. Owens
Sent: Friday, January 05, 2007 12:29 PM
To: [log in to unmask]
Subject: [TN] Solder Designations
Dear Technetters:
I have had a student of mine ask a question which has stumped me, but
should (hopefully) be easy for our metallurgist folks out there.
J-STD-001 3.2 Solder refers to Sn60A, Pb36B and Sn63A. To what specific
solder alloy do these designations apply? I have looked at J-STD-005B to
attempt to find these specific designations (specifically the inclusion
of "A" or "B") but without success.
Any thoughts?
Gregg Owens, MIT
Manufacturing Technology Training Center, Inc.
Mira Loma, CA 91752
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|