TECHNET Archives

April 2016

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Reuven Rokah <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Reuven Rokah <[log in to unmask]>
Date:
Sat, 9 Apr 2016 18:38:09 +0300
Content-Type:
text/plain
Parts/Attachments:
text/plain (54 lines)
Cross sections are needed.
It seems there is a sign if flying probe or test probe...can create a short
by excess power.
בתאריך 8 באפר׳ 2016 19:01,‏ "Steve Gregory" <[log in to unmask]> כתב:

> Good Morning All,
>
> We have an assembly that we build here for a customer that we built for
> some time, over 2,000 assemblies. There have been some failures that our
> customer has had field returns with that are beginning to escalate. There
> have been 12 field failures that we know of. The failures are avionic
> assemblies that have been in the field ranging from 111 days to 472 days.
> The actual failures are internal +12V to -12V shorts and we need to know
> why. I have two failed assemblies here. Here are a couple of external
> photos of a via that shows the short:
>
> http://stevezeva.homestead.com/Internal_Short.jpg
>
> http://stevezeva.homestead.com/Internal_Short_Close.jpg
>
> So my question is, can a lab take these boards and examine them to
> determine what the root cause actually is from the two assemblies that I
> have, or does there need to be more samples? What is the range we should
> expect to pay for this type of analysis?
>
> We're trying to work with our PCB vendor on this issue, but I have also
> been asked by my boss to pursue this with a third party.
>
> Thanks!
>
> Steve
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
> --
>
>
> This email and any attachments are only for use by the intended
> recipient(s) and may contain legally privileged, confidential, proprietary
> or otherwise private information. Any unauthorized use, reproduction,
> dissemination, distribution or other disclosure of the contents of this
> e-mail or its attachments is strictly prohibited. If you have received this
> email in error, please notify the sender immediately and delete the
> original.
>

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2