Hi Guy,
I have your pictures published, here are the links:
http://stevezeva.homestead.com/ddr3-board.jpg
http://stevezeva.homestead.com/ddr3-device2.jpg
Steve
On Mon, Jan 22, 2018 at 8:02 AM, Guy Ramsey <[log in to unmask]> wrote:
> So, is poor solderability like the flu . . .
> We are having a rash of it.
> We identified the EPENIG solder problem as a surface contaminate,
> originating at the board house in the final rinse water.
> We did not get to the bottom of the ENIG problem which I am thinking we
> own.
> Here is why.
> The "black pads" may be found on either the board or the device. I have
> attached a photo of each, one on the board and one on the device package.
>
> These are soldered with a WS Pb-free flux. We have carefully developed the
> profile with a long soak, to minimize the void problems on LGA. Ramp,
> soak, and reflow are all within recommendations of the solder paste
> manufacturer.
>
> Steve can you put these up for me. The problem does seem to be more common
> on the DDR3 memory devices than any of the other BGA types.
>
--
Steve Gregory
Kimco Design and Manufacturing
Process Engineer
(208) 322-0500 Ext. -3133
--
This email and any attachments are only for use by the intended
recipient(s) and may contain legally privileged, confidential, proprietary
or otherwise private information. Any unauthorized use, reproduction,
dissemination, distribution or other disclosure of the contents of this
e-mail or its attachments is strictly prohibited. If you have received this
email in error, please notify the sender immediately and delete the
original.
|
|
|