TECHNET Archives

June 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Genny Gibbard <[log in to unmask]>
Date:
Wed, 2 Jun 2010 18:24:11 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Vladimir Igoshev <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
Subject:
From:
Vladimir Igoshev <[log in to unmask]>
X-cc:
In-Reply-To:
Organization:
SENTEC
MIME-Version:
1.0
Parts/Attachments:
text/plain (40 lines)
Hi Genny,

I don't like guessing. It well could be overheating (as Dave said)
and it could be to an unacceptable degree, so your new joints won't
be reliable whatsoever. I had a case of reworked BGA, where it
received so much heat that Cu pads on the UBM got  dissolved in
solder leaving the balls hanging to the pads only around the
perimeter.

I ALWAYS recommend to do analysis, either prior to repair or after to
confirm the part/assembly is still reliable..

-- 
Best regards,

Vladimir                          mailto:[log in to unmask]

SENTEC  Testing Laboratory Inc.
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2