I have a mixed technology board - bottom side smt  power supply which is 
failing. I suspect that the failure is due to the unreliability of 
decoupling ceramic caps.
On reworking the caps they tend to crack.
I have subjected them to thermal shock tests and they seem to retain their 
 integrity.
Any suggestions? Is it a vendor problem (which seems unlikely) only?
Thanks in advance.
 

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2