TECHNET Archives

March 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Jim Henderson <[log in to unmask]>
Date:
Wed, 31 Mar 2004 16:01:16 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Jeffrey Bush <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Jeffrey Bush <[log in to unmask]>
Parts/Attachments:
text/plain (59 lines)
Several liquid dielectrics are available for laser via formation.
MacDerid makes a Macuvia dielectric that can be used to fill higher
copper topographies and could be then bonded further to complete the ML
package.  I do not know the modulus constraints of the material - a link
to the site is:

http://www.macprintedcircuits.com/advanced/

I know that Ciba makes one or more also -


Jeffrey Bush
Director, Quality Assurance and Technical Support

                          76 Technology Drive - POB 1890
                             Brattleboro, Vermont 05302-1890
                                Tel. 802.257.4571.21 Fax. 802.257.0011
                                    [log in to unmask]
                              http://www.vtcircuits.com	



-----Original Message-----
From: Jim Henderson [mailto:[log in to unmask]] 
Sent: Wednesday, March 31, 2004 11:48 AM
To: [log in to unmask]
Subject: [TN] flex coversheet alternatives


Has anyone heard of an industry accepted LPI flex mask or photoimageable
coversheet.  Squeeze out is becoming a huge problem on 3 oz. cu @ 8 mil
spacing.

Thanks
Jim H.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2