Mornin' Ioan!
You know, that hasn't occured to me. Maybe somebody else that
knows more about metallurgy than I do could answer. I wouldn't think
that would be a huge issue though...I might be wrong.
The point in reballing with 63/37 spheres is to avoid all the voiding
issues with lead free spheres, and to replace them with a alloy that's
better understood as far as performance and reliability is concerned.
Kind regards,
-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
|---------+---------------------------->
| | "Tempea, Ioan" |
| | <itempea@POSITRON|
| | .QC.CA> |
| | Sent by: TechNet |
| | <[log in to unmask]>|
| | |
| | |
| | 06/16/2005 07:45 |
| | AM |
| | Please respond to|
| | TechNet E-Mail |
| | Forum; Please |
| | respond to |
| | "Tempea, Ioan" |
| | |
|---------+---------------------------->
>--------------------------------------------------------------------------------------------------------------|
| |
| To: [log in to unmask] |
| cc: |
| Subject: Re: [TN] NTC-Really, really pretty solder... |
>--------------------------------------------------------------------------------------------------------------|
Hi Stevie Roy,
you might want to keep it NTC, but I see a very technical issue here. This
is the re-balling with 63/37. The original balls were lead-free, therefore
having created some specific intermetallics between the chip and the ball.
If you put the leaded balls on, how reliable will be the new intermetallics
that are formed?
Just a thought.
Regards,
Ioan
> -----Original Message-----
> From: TechNet [SMTP:[log in to unmask]] On Behalf Of Stephen Roy Gregory
> Sent: Wednesday, June 15, 2005 11:02 PM
> To: [log in to unmask]
> Subject: [TN] NTC-Really, really pretty solder...
>
> Hi everyone!
>
> First, I want to express why I posted what I did earlier. I see all this
> "Lead-free" stuff in
> every trade magazine that I pick-up, I get spam email from everywhere
that
> you can imagine, about lead-free seminars, training classes, why I need
to buy
> different equipment, yada-yada-yada.
>
> But then I hear off-the-record from engineers at companies who are our
> customers, that they aren't even thinking about lead-free solders.
>
> I'm starting to look at tinning all components with standard 63/37
solder,
> re-balling BGA's with 63/37 spheres, and every other means available to
meet our
> customer demand to stay away from anything and everything lead-free, and
to
> try and remain competitive. On top of all of this, I will probably have
to
> figure out how to run a lead-free line and keep everything under control
at the
> same time, because we do have customers that will be marketing their
stuff in
> Europe... talk about alligators!
>
> We don't have a big engineering staff, or a nice lab to do experiments or
> analysis. We're not unlike a lot of EMS companies our size. We're a high
mix, low
> volume shop that specialize in defense and military electronics, that's
our
> heritage. We do things in the way that has been proven, and known to be
> reliable. When this lead-free deal was put on the table, it has turned
things upside
> down for me at least. I guess I was just trying to find out if anyone
else
> felt as p*ssed off as I am and as overwhelmed about lead-free as I do.
>
> On a lighter note, but in the same vein though, I took a cue from an
earlier
> post, and have created an image on my web page of what Tin/lead solder
might
> appear as in the year 2010.
>
> Take a look at: http://www.stevezeva.homestead.com , go to Picture Page
2,
> and look at; "REAL Pretty Solder".
>
> -Steve Gregory-
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc. It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone. In such event, you should destroy the message and
kindly notify the sender by reply e-mail.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|