TECHNET Archives

November 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Matt Stanik <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Fri, 2 Nov 2001 12:50:21 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (108 lines)
Beck Chemicals Inc.
3350 W 137th St.
Cleveland, OH 44111
(216) 941-8355

EPOXYSTRIP T-251-C
cold stripper, immersion type, thin liquid for stripping epoxies, vinyls,
enamels from steel, copper wire, aluminum, electrical components

EPOXYSTRIP T-251-G
cold stripper, immersion type, no phenolic, same as T-251-C but specially
for use where towns use central septic sewage or rural areas where septic
tank sewage serves plants

EPOXYSTRIP T-253-F
cold stripper, immersion type, extra strength for straight epoxies and
alkyds

EPOXYSTRIP B-251-CW
Brush type, for removing heavy duty finishes on metal

Last time I used the product was mid 90's, so you may
have to check into current availability.





-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Marsico, James
Sent: Wednesday, October 31, 2001 12:11 PM
To: [log in to unmask]
Subject: Re: [TN] STRIPPING MAGNET WIRE


Can't find ant info on Beck chemicals (EPOXYSTRIP T-251-C) or Insulstrip
Jell.  Do you have any additional information?

Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879



        -----Original Message-----
        From:   Matt Stanik [SMTP:[log in to unmask]]
        Sent:   Wednesday, October 31, 2001 12:46 PM
        To:     [log in to unmask]
        Subject:        Re: [TN] STRIPPING MAGNET WIRE

        Beck Chemicals of Cleveland, Ohio used to sell a product called
        EPOXYSTRIP T-251-C specifically for removing insulating varnishes
        and epoxies from wire and such. It worked great.


        > Looking for a recommendation for a chemical stripper to strip
bi-filar (?)
        > magnet wire.  Any suggestions?
        >


----------------------------------------------------------------------------
-----
        Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt delivery of Technet send the following message:
SET Technet NOMAIL
        Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
        Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
        information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315

----------------------------------------------------------------------------
-----

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2