Ketan ,
with only a few of PTH's yo' right, saves time, as long as you have decent
welders.
I would not solder upside > solder runs down the component too readily ,
flooding/swelling the legs, it's a mess .
Solder from PTH components side , with legs properly trimmed ,
than you have no problems , good heat approach, full barrel.
Needless to say a tear of solder on iron will get you there faster,
operators have a bad habit of keeping tip dead/"clean"/dry/cold,
by ever so diligent wipes !
Feed wire between leg and tip poked to hole,
some of the handsoldering seen would give Jim fits,
never just assume it's simple enough > it ain't .
Desire of add flux abolishment is indeed commendable .
ave a goood wknd pk
-----Original Message-----
From: Ketan Bhatt [mailto:[log in to unmask]]
Sent: Friday, 18 August 2000 15:32
To: [log in to unmask]
Subject: [TN] Manual soldering of PTH joint from component side.
Hi TechNetters !!
I am facing a typical problem. Our boards have 80~90 smt components on them
and all are on one side. Balance of PTH components are on both the sides so
after reflow, we use manual soldering. I am looking forward to do manual
component insertion and soldering from component side to save time. My
question is - Is it the right way to solder the component from comp side?
How do we ensure proper filling of PTH and proper joint at solder side? We
are using no-cleaned cored solder wire from Kester. Presently we are using
additional flux but I want to eliminate it.
Looking forward to your answer. Thank you in anticipation.
Bye,
Ketan Bhatt
Secure Meters Limited.
India.
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|