1st picture is very interesting...
2nd picture looks like an overvoltage problem. Tantalums have a problem
with operating near rated voltage over time/temperature. Anymore we
spec tant rated volts at 2 times the operating voltage (where we can) to
avoid this problem.
3rd picture would make for a great hot dog roast!
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Friday, September 08, 2006 10:50 AM
To: [log in to unmask]
Subject: Re: [TN] Tantalum Caps
Hi Dave!
Yes it's FRIDAY!! (Thank goodness!!) I got your picture and it's posted.
Pretty "dramatic" all right...looks like the thing turned itself inside
out! check out:
http://stevezeva.homestead.com/files/Daves_Tantalum.jpg
I had another picture sent to me that's just as "dramatic". But I think
that this one shorted somehow or was put on backwards...almost blew the
traces off the board! Look at this one:
http://stevezeva.homestead.com/files/Crispy_Tantalum.jpg
Then there's another picture. This one is almost beyond
desciption...check out:
http://stevezeva.homestead.com/files/Real_Crispy_Tantalum.jpg
I wouldn't want to even be around that one, that's for sure!
-Steve Gregory-
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Friday, September 08, 2006 7:35 AM
To: [log in to unmask]
Subject: Re: [TN] Tantalum Caps
Hi Steve! It must be Friday if we are discussing exploding components!
Kemet has an very good summary of what can happen to Ta capacitors - in
short they can have a self sustaining metal oxide fire! Here is the
Kemet
reference: Kemet Electronics Corporation Tantalum Applications Notes,
Surge Step Stress Testing in Tantalum Capacitors, 05/03/00. And I'll
send you a much more "dramatic" photo to post! All components have
limits and Ta caps are no exception.
Dave Hillman
Rockwell Collins
[log in to unmask]
stephen gregory
<stephengregory58
[log in to unmask]>
To
Sent by: TechNet [log in to unmask]
<[log in to unmask]>
cc
Subject
09/07/2006 06:17 Re: [TN] Tantalum Caps
PM
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
stephen gregory
<stephengregory58
[log in to unmask]>
Hi John!
Certanly can! They can literally EXPLODE!! I have a graphic example of
that with a picture that was sent to me some time ago when I asked about
Tantalums being moisture sensitive. Check out:
http://stevezeva.homestead.com/files/Rpt_Molded_Tant.jpg
This is what a tantalum looked like after it came out of reflow!!
-Steve Gregory-
John Foster <[log in to unmask]> wrote:
Can Tantalum Caps suffer from popcorning?
Can tant caps absorb enough moisture to cause this type of effect.
We just built some new boards and we have one particular part number
tant that is shorting out left and right.
any input will be appreciated thanks
John Foster
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|