Ken,
I don't know how your test plan is set up, but artificial aging
characteristics (to simulate storage) would be an interesting comparison.
Also planarity if you are using surface mount.
Ralph
> ----------
> From: Ken Patel[SMTP:[log in to unmask]]
> Reply To: TechNet E-Mail Forum.;Ken Patel
> Sent: Wednesday, September 02, 1998 1:39 PM
> To: [log in to unmask]
> Subject: [TN] What to compare for HASL v/s OSP
>
> Surface Finish Experts,
> I am planing to run 50 boards with OSP Coating (Entech) on experimental
> basis before we change from current HASL processed boards. My management
> has
> asked to make a presentation after both HASL and OSP went through assembly
> process. Can anyone suggest me what can I compare besides yield?
>
> re,
> Ken Patel
> ______________________________________________________
> Ken Patel Phone: (408) 490-6804
> 1708 McCarthy Blvd. Fax: (408) 490-6859
> Milpitas, CA 95035 Beeper: (888) 769-1808
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|