Hi Cheryl,
We have a similar requirement currently in-process that we are completing
for a customer. We are using a precision drill system with a drill to ream
the holes and remove the majority of the solder to allow the press fit pins
to be inserted. It does require investigating the board design to confirm
the original hole drill size, and the plated hole wall thickness. Give me a
call if you'd like to discuss further.
Andy Price
Sales Manager
978-374-5000 ext: 18
PS. Keep up with the latest industry news, and learn some
Tricks-of-the-Trade we've discovered over the past 20 years. All of this and
more in the Circuit Technology Center eNewsletter. See the latest issue at
http://www.circuittechctr.com/general/enews.shtml. Visit the bottom of the
newsletter for a free subscription.
-----Original Message-----
From: Crepeau, Phil [mailto:[log in to unmask]]
Sent: Monday, August 09, 2004 4:38 PM
To: [log in to unmask]
Subject: Re: [TN] Removing solder from PTH barrels
hi,
i don't know the exact conditions of your pwb, but might it not be possible
to run it through a solder dip and hot air leveling operation?
phil
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Cheryl Tulkoff
Sent: Monday, August 09, 2004 12:45 PM
To: [log in to unmask]
Subject: [TN] Removing solder from PTH barrels
Does anyone have any clever suggestions on how to get solder (all of it)
out of .024" diameter PTH barrels?
The barrels are supposed to be completely clear of solder since they are
used for a press-fit connector. There is just enough solder in the holes
to keep the connectors from seating properly. The barrels ended up with
solder paste in them after some boards were run using the wrong stencil.
The operator wiped the boards by hand towards the holes forcing some
solder paste into the barrels. He didn't follow up with a clean either.
While I'm at it, does anyone have a really good process for cleaning
misprinted boards? Obviously, our current procedure wasn't followed but
maybe someone has a better way.
Thanks, Cheryl
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|