TECHNET Archives

September 2002

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Sasha Miladinovic <[log in to unmask]>
Date:
Wed, 25 Sep 2002 08:56:57 -0700
MIME-version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Dan R. Johnson" <[log in to unmask]>
Content-type:
text/plain; charset=iso-8859-1
Subject:
From:
"Dan R. Johnson" <[log in to unmask]>
Content-transfer-encoding:
7BIT
Parts/Attachments:
text/plain (17 lines)
*Caution* use a "Pink Pearl" type eraser, the type used for ink will remove
the gold plate. (He remarked sheepishly.) Yes, this is the voice of
experience. I learned this lesson in the eighties building/repairing traffic
controller modules.
Dan

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2