TECHNET Archives

February 2014

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Whittaker, Dewey (EHCOE)
Date:
Thu, 20 Feb 2014 19:01:31 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (47 lines)
They always said that process had no margarine for error.
Dewey

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Thursday, February 20, 2014 11:49 AM
To: [log in to unmask]
Subject: Re: [TN] Acetone as a cleaning agent for PCBA's

It can remove the resin buttercoat, and if left on it can penetrate into the soldermask bond and then ultimately into the resin bond of the FR-4 itself. Acetone is also known to dissolve certain polymers, especially diallyl phthallate (sp) and other connector body plastics, and will completely cloud over LED lens and other materials. It can cause some conformal coatings to swell up, so badly that the chip resistors and caps with conformal coating underneath will crack in half. 
And it is especially bad for pregnant mothers-to-be, as it can cause the child to be born completely bare-naked and sometimes even bald! I once asked my mother if that is what happened to me, and she said "No, honey. Grass just does not grow on a busy street. " 

To which my Dad observed, "Doesn't grow on a cement block either, son".


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Larry Dzaugis
Sent: Thursday, February 20, 2014 12:34 PM
To: [log in to unmask]
Subject: Re: [TN] Acetone as a cleaning agent for PCBA's

It will wipe off non epoxy ink markings.
Dissolve other materials that may not have been touched by your aqueous cleaner chemistry.
Leave a haze if not wiped off.

Remember Chem Lab and using it to clean test tubes?
Took some practice to end up with a clean test tube.

More flammable than IPA.

>
> Larry Dzaugis


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2