TECHNET Archives

September 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Pasquito, Helena" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Pasquito, Helena
Date:
Fri, 23 Sep 2005 10:39:32 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (60 lines)
Hi All,

There is a great paper by Bob Willis on fillet lifting.  Check out his website: www.leadfreesoldering.com.  

Regards,
Helena Pasquito  

 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Roland Dollinger
Sent: Friday, September 23, 2005 5:39 AM
To: [log in to unmask]
Subject: [TN] lead free soldering "fillet lifting"

Dear all,

who has detailed info for me about lead free soldering due to "fillet lifting"

What is the root cause of fillet lifting?
- Low cooling rate after soldering?
- contamination of Bi?
- contamination of Pb?
- amount of latent heat released during solidification?
- Does fillet lifting not occurs, when the FRI (fillet-lifting resistant
index) is bigger than 0,75?

How can we avoid fillet lifting?

Has anybody read the US patent US6617529A1_anti solder fillet lifting?
This patent recommend a pad width bigger than 0,4mm to avoid fillet lifting. Does everybody know, what this patent will mean for us?
I read the old aged MIL-STD-275E and in my opinion I´m convinced, that due to this MIL standard the US-patent US6617529A1is covered too.
What do you think about this?

Thank you for your comments.

Roland Dollinger
Valeo
Process Engineer
Valeostraße 1
86650 Wemding
Germany

[log in to unmask]


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2