TECHNET Archives

March 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Ingemar Hernefjord (KC/EMW)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Ingemar Hernefjord (KC/EMW)
Date:
Mon, 7 Mar 2005 07:57:28 +0100
Content-Type:
text/plain
Parts/Attachments:
text/plain (65 lines)
agree. We had a p-p with an odd behaviour: up and then, components just disappeared. We scratched our heads and knees, creeping under the machine to look for the vanished creeps. Finally,  a guy decided to go to the bottom with the mystery, and he started disassemble the machine. In a non inspectable part of the machine he found a plate full of chips, hundreds of them, electrostatically catched by the paint of a plate.

Ingemar Hernefjord
Ericsson Microwave Systems

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]
Sent: den 4 mars 2005 16:39
To: [log in to unmask]
Subject: Re: [TN] Machine surface treatment for ESD and good looks


I see a conductive surface as superior to a "dissipative" one, although not
as cosmetically acceptable in your case.


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Evans
Sent: Friday, March 04, 2005 10:28 AM
To: [log in to unmask]
Subject: [TN] Machine surface treatment for ESD and good looks

I have an issue concerning worn out machine surface coatings. I have a
MyData that has what looks like a conversion coating on the Y-Wagon that has
worn through to a near shiny metal surface. This same kind of coating has
been applied to other machines and like the Mydata, they are also worn out.
The problem with this is that the surface has become conductive and now has
a direct path to ground. When the machine was new, the coating had created a
disipative surface.  I want to restore this original effect of a disapative
surface and possibly restore the lovely lustre of the original finish.
Anyone out there been down this road?

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2