TECHNET Archives

December 2010

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Laroe, Michael" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Laroe, Michael
Date:
Mon, 6 Dec 2010 16:58:23 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (82 lines)
Thanks Kevin..

The Solders were chosen after a DOE was done on each comparing them to others alike approx 7yrs ago. We also restrict the operators from using additional flux so that the remaining material left behind has definitely seen temps well above 170oC.. Knowing this I know the flux left behind is definitely benign.  However, if additional flux is absolutely needed then there are specific cleaning instructions to ensure nothing corrosive, conductive is left behind.  Also, the Kester Flux core we are using is the 66 which contains 3.2% Flux content which allows a much better flow than the standard 2%..

Given this can you see any other reason not to use the Kester for both requirements.

Thanks again,

Mike

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Glidden, Kevin
Sent: Monday, December 06, 2010 4:51 PM
To: [log in to unmask]
Subject: Re: [TN] HandSoldering Using NC Solders

Mike,
That's a big one.  The answer is that you need to choose the best solder(s) for your application(s).  It is likely your two solders were selected by two different people at two different times.  When choosing materials, talking to the manufacturers about the products, getting samples, and comparing them head-to-head goes a LONG way.  You must also consider reliability.  The best flux formulation is simply not the one that allows you to solder a rusty nail to the hull of a ship.  An important factor is how you plan to clean your parts after soldering is all done, how well you can ensure you get all the residues removed, and the potential impact of any residues remaining on the assemblies.  I suggest you start by reading through some tech articles on cleaning.  This forum, the industry magazines, Foresite, and ACI are some good starting resources.  Bottom line - you don't pick solder materials solely on the basis of supplier or cost.
Good luck.

-----Original Message-----
From: Mike Laroe [mailto:[log in to unmask]]
Sent: Monday, December 06, 2010 4:06 PM
To: [log in to unmask]
Subject: [TN] HandSoldering Using NC Solders

Currently my company has been using two different Alloys for handsoldering
both Leaded and RoHs No-Clean Assy's.  For the leaded requirement we are
using AIM and for Rohs we are using Kester.  We currently stock 4 different
sizes of each (.015", .020", .025", .031")..  My question and thought is to
phase out the AIM and strictly only use the Kester for both Leaded and Rohs
Assy's.  All the Soldering is done with Metcals using the 700 & Pwr Tips.  Are
there any reasons I shouldn't do this?

Thanks for your help in advance,

Mike Laroe
Mfg Engineer

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

WARNING: Export Control
This message, including any attachments, may contain technical data within the definition of the International Traffic in Arms Regulations (ITAR), and subject to the Export Control Laws of the U.S. Government. Transfer of such information by any means to a foreign person, whether in the United States or abroad, without proper export authorization or other approval from the U.S. Department of State is prohibited.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2