TECHNET Archives

April 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Martin Butcher <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Martin Butcher <[log in to unmask]>
Date:
Tue, 19 Apr 2005 15:29:03 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (29 lines)
Hi All,

I have a question regarding the discoloration of the silk screen ink after
reflow.  What can cause it other than overheating during reflow?

Here is some background to this question.  We received a consigned kit,
processed it and shipped it about three months ago.  Our profile data shows
that the PCB did not reach peak temperatures above 216 deg C.  We have run
this product once prior with a peak temperature of 212 deg C and with no
reports of discoloration.

Our client has contacted their board shop concerning this and were told by
the board shop that the discoloration is due to overheating.  Are there
other variables that could account for this?

Regards,
Martin Butcher,
Process Engineer.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2