TECHNET Archives

July 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Wayne Thayer <[log in to unmask]>
Date:
Thu, 17 Jul 2014 23:36:29 +0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Tuyen Tran <[log in to unmask]>
Message-ID:
Subject:
From:
Tuyen Tran <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (51 lines)
Wayne

Yes, the staining on ground plane not affect 3F, because it were not soldered so it were stained during production time and looked so bad about cosmetic. Can you advise how to treat of stain? We not confident to delivery to customer these boards.

Thanks
Tuyen Tran

________________________________________
From: TechNet [[log in to unmask]] On Behalf Of Wayne Thayer [[log in to unmask]]
Sent: Thursday, July 17, 2014 10:57 PM
To: [log in to unmask]
Subject: Re: [TN] Staining immersion silver coating on ground plane after assembling

What's to solve?

Apparently the boards soldered OK, so it sounds like you are only talking
about cosmetics. No long term reliability problem.

Talking with the PCB supplier about getting an anti-tarnish applied over the
ImAg will help with the cosmetics.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tuyen Tran
Sent: Thursday, July 17, 2014 11:42 AM
To: [log in to unmask]
Subject: [TN] Staining immersion silver coating on ground plane after
assembling

Hi Everyone
We received some PCBs where the finish surface was good, but after we ran
reflow about ten days, the ground plane with immersion silver coating that
were not covered by solder paste look to be stained on surface.
We known the chemical silver [Immersion Silver finish] surface is very
sensitive to surrounding condition, it is easy to stain from oxygen/water
vapour or production time exposure in the air.
We are looking for document on staining metal of the finished board. Has
anyone else experienced something similar phenomenon or anyone have an idea
to solve this?
Thanks
Tuyen Tran.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2