TECHNET Archives

June 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Bobby R. Mangona" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Mon, 1 Jun 1998 13:09:08 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (24 lines)
------- Forwarded Message Follows -------
From:          Self <bobby>
To:            TECHNET
Subject:       Termination Loss
Date:          Sat, 30 May 1998 08:45:51

We are experiencing termination loss of chip capacitors and chip
resistors after the reflow process.
Can anyone told me the possible causes?
Is it a material related problem?Since we have already checked the
reflow profile and found to be within specification.

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2