About 3 months ago we converted our manufacturing system from RA flux to OA
flux. Along with the conversion we switched from a solvent board wash to an
aqueous board wash using closed loop DI water only. Now I have people
complaining that the solder wick (un fluxed) I switched to doesn't work well
at all. I have suggested that they need to use some of the liquid OA flux
that they have been supplied, but still people are unhappy. A few
assemblers had used a no-clean flux solder wick with a previous employer,
which seemed to work well. My question is are there wash/compatibility
problems with this no-clean flux wick, my DI water wash system and residue
left on the boards after wash?
Phil Nutting
Manufacturing Engineer
Kaiser Systems, Inc.
978-922-9300
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|