Roger, sometimes when common criteria is used in more than one document
we have to deal with the leapfrog effect.
610C addresses wires that are to be soldered. A-620, which is targeted
for cable/wire harness mfg, was published several years after 610C.
A-620 had a need for expanded coverage because the soldering process can
compensate for some strand damage that would lead to premature failure
in a crimp connection.
The 610 committee (and the J-STD-001 committee), when building revision
D of these documents, made the decision to include a more complete table
such as that in A-620. In the process, these two commitees worked with
the A-620 committee to resolve some concerns in the criteria. When 620
Rev A (expected to be balloted in the spring) is published, the strand
damage tables in all three documents will align.
Jack
Jack Crawford, IOM
IPC Director Certification and Assembly Technology
[log in to unmask]
NEW PHONE 847-597-2893
NEW FAX 847-615-5693
IPC HAS MOVED- NEW ADDRESS:
3000 Lakeside Drive, Suite 309 S
Bannockburn, IL, 60015
New main Phone 847-615-7100
New main fax 847-615-7105
Check www.ipc.org/move for new staff phone numbers.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Roger Mack
Sent: Tuesday, December 14, 2004 3:17 PM
To: [log in to unmask]
Subject: [TN] wire strand damage tables don't match
IPC-610C table 5-4 identifies the number of allowable damaged strands in
a wire. This table does not match the one in IPC/WHMA-A-620 table 3.1
(page
3-2)
Is there a plan to align these tables in the upcoming revisions of these
documents?
Roger Mack
Manufacturing Engineer
Vansco Electronics LP
Winnipeg, Manitoba
Canada,
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|