TECHNET Archives

March 2013

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Richard D. Krug" <[log in to unmask]>
Date:
Wed, 13 Mar 2013 11:04:17 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
"David D. Hillman" <[log in to unmask]>
Message-ID:
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (45 lines)
Hi Dick - what is the solder paste container: a SEMCO type tube or a jar?

Dave Hillman
Rockwell Collins
[log in to unmask]



From:   "Richard D. Krug" <[log in to unmask]>
To:     <[log in to unmask]>
Date:   03/13/2013 07:42 AM
Subject:        [TN] Cooling of Solder Paste Overnight
Sent by:        TechNet <[log in to unmask]>



It has been proposed that we take left over solder paste and store at ~60 
F overnight to extend life and integrity of paste.  This would be paste in 
its original tube or jar, not recovered from a stencil.  We are located in 
Florida.  During the summer, when the AC is reduced overnight, temperature 
in the building gets to ~85 F. 

Has anyone done this?  What are the pro's and con's? 

Dick Krug, CSSBB, CSMTPE
Senior Process Engineer
Sparton Complex Systems
30167 Power Line Road
Brooksville, FL  34602-8299
p (352) 540-4012  (Internal Ext. 2012)
[log in to unmask]

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2