We assemble PCB for space applications so it is clearly a class 3 board.
And we are allowed to rework one time each solder joint. So that means that
every joint can be touched up one time.
After, we have to change the component.
So, I think you customer has missed something !
Vincent Bada
Process Engineer
Alcatel ETCA
Belgium
mike connolly <[log in to unmask]> le 25/09/2000 14:28:10
Veuillez répondre à "TechNet E-Mail Forum." <[log in to unmask]>; Veuillez répondre
à mike connolly <[log in to unmask]>
Pour : [log in to unmask]
cc : (ccc : Vincent BADA/ETCA/ALCATEL-SPACE)
Objet : [TN] IPC-R-7221
Fellow Technets,
A question was posed to me by a customer claiming that
IPC-R-7221 stated that a maximum of 1 rework per board
for class 3 was acceptable. Specifically they stated
that this means only 1 solder joint per board could be
touched up. I have been searching high and low for
IPC-R-7221 but to no avail have yet to find the
existence this publication.
My questions are:
1. Does IPC-R-7221 exist?
2. If so, can anyone support or refute the claims of
only being able to touch up 1 solder joint on a class
3 assembly?
Any help or input would be appreciated.
Best regards,
Mike
__________________________________________________
Do You Yahoo!?
Send instant messages & get email alerts with Yahoo! Messenger.
http://im.yahoo.com/
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|