TECHNET Archives

September 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Jim Marsico 516-595-5879 <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Tue, 29 Sep 1998 08:00:00 -0400
Content-Type:
TEXT/PLAIN
Parts/Attachments:
TEXT/PLAIN (41 lines)
Are these "dimpled" BGAs?  Are the component pads recessed below the bottom
surface?  If so, perhaps you might try screening the flux instead of
dispensing.  This might give you a better flux deposit without voids.

Jim Marsico
AIL Systems Inc.
(516) 595-5879
[log in to unmask]



Fumiaki Shigeoka wrote:

My problem is dropping solder ball from BGA devices after ball attachment
process.
First, I suspected the temperature of reflow oven, but that was sufficient to
melt
solder ball. After reflow, some balls(5-10% of strip) are missing, and empty
pads
are not wetting or partially wetting.
I found voids in flux on pad before placing ball, so I guess the void will
expand
in reflow furnace, and ball doesn't touch to pad. I use dispensing system to
provide
flux, which sometimes contaminates air void to flux on pad.
Does anyone have any experiences and suggestions to solve this problem ?

Thanks in advance.

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2