Hi,

Interesting question. The only thing which comes to mind is this. The
stencil is 6mm thick. Then logic says you will get 6mm of paste. We use
metal squeegees with metal stencils for years and have good results. The
only thing is if Vendor 1 boards pads are as wide and the stencil holes.
Then you should get 6mm of paste. But if vendor 2's pads are wider then the
PCB is not flush with the stencil. The paste on the pads still will be 6mm
but maybe the pads on the board are wider and not hot air leveled so
good????? Just my 2 cents. Have a great week.

John

At 09:57 PM 6/26/99 , you wrote:
>Hi,
>
>Have anyone encountered that PCB from different suppliers give different
>paste height.
>
>We are using 3 PCB suppliers for one of our product, and the average paste
>height we are getting (on 2 suppliers), using 6 mil stencil with rubber
>squeegee (70 durometer) gives an average paste height of 6.5 mil. However,
>there is one supplier's PCB that gives the average paste of 8 mil.
>
>We need to double the squeegee pressure to achieve the paste height of near
>7.0 mil
>
>Could anyone advise me the cause to such issue.
>
>Thanks
>
>Poh
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe:   SUBSCRIBE TechNet <your full name>
>To unsubscribe:   SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2