Ok, I'm probably showing my ignorance here,
but with a stable non-corrodable finish like
Sn-Ni, why do you need the gold?
Jack (a PCB layout guy)
Automatic digest
processor
<LISTSERV@LISTSER
V.IPC.ORG>
Sent by: TechNet To: Recipients of TechNet digests <[log in to unmask]>
<TechNet@listserv cc:
.ipc.org>
05/23/2003 12:00 Subject: TechNet Digest - 21 May 2003 to 22 May 2003 (#2003-154)
AM
Please respond to
TechNet
Caterpillar: Confidential Green Retain Until: 06/22/2003
Retention Category: G90 -
Information and Reports
----- Message from Happy Holden <[log in to unmask]> on Thu, 22 May 2003
08:44:12 -0400 -----
Subject: Re: Sn-Ni PCB
plating
Tin-Nickel alloy plating is a unique metal that is just about uncorrodable.
We used it at Hewlett-Packard for about 23 years (1965-1988). First as a
final finish (but in those days we had acid fluxes in the wave solder) than
as a barrier metal under bright tin and then gold. You can read about it
in Coomb's PC Handbook 4th Ed. (pp. 19.42-19.44) or earlier. It is not in
the new 5th Ed. I don't know if it is being used anymore in the San
Francisco Bay Area like in the earlier days of pcb growth. It is a
non-proprietary plating bath that has no organic additives. It can be
difficult to control and its plating can be very stressed. But it has a
number of unique metallurgical properties--It is non-magnetic--Gold WILL
NOT DIFFUSE INTO IT--It will not corrode unless you use concentrated
aqua-regia. Stanford Univ once did a project to understand how the alloy
worked because the properties were SO MUCH different from either nickel or
tin. The report was fascinating, especially for a metallurgist because the
alloy was truly unique.
Morton Adler of Bell Labs did a lot of research on it because 5 microinches
of gold on tin-nickel out performed their 100 microinches of gold on nickel
for switch contacts.
I think Electrochemicals developed a proprietary tin-nickel that had an
organic stress reducer in it and did not require hydrofluoric acid to
control the pH. The Metal Finishing Handbook had the bath formulation in
it. I know personally that it made a great finish for sail boat
parts--never a sign of salt water corrosion in 20 years and we helped some
artists in Estes Park, COL plate a bronze statue so it would look good
forever.
Happy Holden
Westwood Associates
375 Morgan Lane, #206
West Haven, CT 06516
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|