     I recently purchased the text "Solder Mechanics-A State of the Art 
     Assessment" for a very reasonable $10.00, published by the TMS 
     technical society, edited by D. Frear, W. Jones, & K. Kinsman,      
     424 pp., 1991.
     I believe you can order the text via the TMS web site.
     
     According the Pb-Sn equilibrium phase diagram on pg. 2, the eutectic 
     is at
     
     61.9 wt.% Sn, @ 183 deg C, or- 73.9 atomic % Sn.
     
     The cited refence for this diagram is:
     
     I. Karakaya & W. T. Thompson, Bull. Alloy Pha. Dia., 1988, vol. 9, 
     pp.144-152
     
     [log in to unmask]
     Lockheed Martin


______________________________ Reply Separator _________________________________
Subject: Re: Sub: Solder Paste Plastic or Eutectic
Author:  [log in to unmask] at _internetcc
Date:    11/23/96 1:02 PM


Dave, you said:
     
     
>     The true
>     eutectic for tin/lead is 61.9%tin/38.1%lead (183C)- everyone calls 
>     63/37 or 60/40 eutectic but they are really near eutectic alloys.
     
Hmmm.  I have seen dozens of references which show 63.0%/37.0% to be the 
eutectic composition for tin-lead binary alloys, and this is the first time 
I've seen otherwise.
     
Anybode got a new edition of Hansen? I'd like to see confirmation, 
otherwise I'll keep my solder post as close as possible to 63% tin. We'd 
all be able to save some money if you are!
     
     
regards,
     
Jerry Cupples
Interphase Corporation
Dallas, TX USA
http://www.iphase.com
     
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To unsubscribe from this list at any time, send a message to:           * 
* [log in to unmask] with <subject: unsubscribe> and no text.        * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2