TECHNET Archives

September 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Franklin Asbell <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Franklin Asbell <[log in to unmask]>
Date:
Thu, 8 Sep 2005 12:13:02 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (98 lines)
That's where my thought was headed until I received more information from
the customer.

Order qty was 99 pieces. They process in 6 piece lots and 2 of them from the
most recent lot ran turned that color. The others had no issues.

There are 15 pieces per panel fabricated.

I've left messages at Cookson/Enthone...so if any of you technicians are
viewing this please call and help solve this puzzle.

Franklin

-----Original Message-----
From: Wolfgang E. Erat [mailto:[log in to unmask]]
Sent: Thursday, September 08, 2005 11:54 AM
To: [log in to unmask]
Subject: Re: [TN] Pink symbol ink...

insufficient cure of the ink could do this

Wolfgang

----- Original Message -----
From: "Franklin Asbell" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, September 08, 2005 12:38 PM
Subject: [TN] Pink symbol ink...


> We got a call from a customer expressing an interesting issue.
>
>
>
> They ran product through their wave solder and the symbolization went from
> white to pink.
>
>
>
> I've never heard of this color change appearing, anyone out there have an
> idea?
>
>
>
> The symbol is Enthone 50-100R - white, the wave solder info I have is Type
> R
> flux with a peak temperature of 215 C.
>
>
>
> Appreciate any input, thanks.
>
>
>
> Franklin
>
> pI
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2