We have problem from time to time also.  I'm trying a new light ring on a
Panasonic MPA-80 that is supposed to help this problem.  I'll try to get a
response out in a few weeks after I see what improvement it makes.  

P.S.  It might help to state what machine types you have when asking for
help on specific issues.


At 05:52 AM 3/12/97 -0500, you wrote:
>>Return-Path: <[log in to unmask]>
>>Resent-Date: Tue, 11 Mar 1997 22:19:09 -0800
>>Resent-Sender: [log in to unmask]
>>Old-Return-Path: <[log in to unmask]>
>>From: Darrell Daigle <[log in to unmask]>
>>To: ipc <[log in to unmask]>
>>Subject: FIDUCIALS
>>Date: Tue, 11 Mar 97 16:28:00 PST
>>Encoding: 7 TEXT
>>Resent-Message-Id: <"oxqT7.0.IiF.NlS9p"@ipc>
>>Resent-From: [log in to unmask]
>>X-Mailing-List: <[log in to unmask]> archive/latest/11033
>>X-Loop: [log in to unmask]
>>Resent-Sender: [log in to unmask]
>>
>>
>>Hello Technetters,
>>
>>I am having a slight problem with the amount of solder on fiducials. This is 
>>causing optical recognition problems during the pick and place.
>>
>>Any suggestions, maybe an alternative surface finish.
>>
>>***************************************************************************
>>* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
>>***************************************************************************
>>* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
>>* with <subject: subscribe/unsubscribe> and no text in the body.          *
>>***************************************************************************
>>* If you are having a problem with the IPC TechNet forum please contact   *
>>* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
>>***************************************************************************
>>
>>
>>
>----------------------------------
>Jeffery L. Hempton              Phone: (219) 429-7335   Fax: (219) 429-4688
>Boardshop Manufacturing Engineer			Mail Stop: 25-31
>Hughes Defense Communications                           
>1010 Production Road, Fort Wayne, IN 46808-4106
>Email: [log in to unmask]
>
>"Those who dream by day are cognizant of many things which escape those who
>dream only by night"    - -Edgar Allen Poe
>
>
>
----------------------------------
Mark W. Spitnale                Phone: (219) 429-5992   Fax: (219) 429-
Hughes Defense Communications                           Mail Stop: 25-31
1010 Production Road, Fort Wayne, IN 46808-4106
Email: [log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2