Susan,
based on my knowledge, the SMT adhesives are normally epoxy base (thermoset
type, not move after curing)...If you see the adhesive got inside the crack
of a resistor, is it possible that coating material of resistor (the
resistor should be caught by electrical testing from the vendor) or coating
material of the assembly get into the crack? (thermal plastic adhesive
normally are not used as SMT adhesive, not to my limited experiences)
...However, if someone is using curing SMT adhesive and reflow in one step
(as cost saving measure...I heard about this...didn't like it a bit)....it
is possible to get cracked during the modified process.
The other place to look is the pick and place machine. It could crack the
resistor upon placing...You will have the SMT adhesive fill up the crack at
placing time (it is liquid form at that stage..).
good luck...
jk
At 11:26 AM 10/11/99 EDT, you wrote:
>Hi All
>Does the "cured" adhesive used to secure surface mount components
>to the bottom - wave solder - side of a board flow during wave solder
>operations?
>
>I am trying to find out how/when the adhesive got inside the crack on a
>cracked
>resistor. My impression was that the cured adhesive would not move????
>
>Susan Mansilla
>Robisan Lab
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|