Hi Richard
I understand. There is a real fine line between damage and removal on
both chemical and abrasion removal. I guess it comes down to the care of
the operator, the time they have to do the job and if its worth it
commercially.
Best Regards
Lee Hitchens
Technical Director
SCH Technologies is a Division of SCH Services Limited
Mob: +44 (0) 7862 25 33 21 www.conformalcoating.co.uk
TECHNICAL SUPPORT SERVICE
SCH Services Ltd offers a Technical Support Helpline to help address all issues relating to reliability. This includes contamination testing, cleanliness and cleaning issues, plus any coating related questions.
Please contact us via email or telephone:
[log in to unmask] +44 (0)1226 249019 (office hours & answerphone) +44 (0)7862 253321 (out-of-hours emergency)
The opinions expressed in this e-mail are strictly those of the sender and not of SCH Services Limited. This communication may contain information which is confidential and may also be privileged. It is for the exclusive use of the intended recipient(s). Unauthorised use, copying or disclosure of any of it may be unlawful. If you are not the intended recipient(s) please note that any distribution, copying or use of this communication or the information in it is strictly prohibited. If you have received this communication in error please notify us by e-mail or by telephone (+44 (0)1226 249019) and then delete the e-mail and any copies of it. Virus Warning - Although steps have been taken to ensure that all email and attachments are virus-free, we cannot guarantee nor be held liable.
Company Registration: 04043334
Registered office: SCH Services Limited Newburgh Building McLintock Way Barnsley South Yorkshire S70 6BF
On 30/05/2013 20:59, Richard Kraszewski wrote:
> Thanks Lee.
>
> I have admit that at numerous times I have tried to convince myself that abrasion is a good solution, but actual results have always convinced me otherwise.
> Still do not feel comfortable letting an operator loose with such a tool in one hand and a PCA in the other, No matter how many controls or poke yokes I put into place.
>
> Rich Kraszewski
> (920)969-6075
>
> -----Original Message-----
> From: Lee Hitchens [mailto:[log in to unmask]]
> Sent: Thursday, May 30, 2013 3:24 AM
> To: TechNet E-Mail Forum; Richard Kraszewski
> Subject: Re: [TN] UV Coating Stripper Recommendation Request
>
> Hi Rich
>
> Have you considered the alternate options of abrasion removal? Something
> like Crystalmark's systems?
>
> is it a large area or a small area to repair? Since it is Uv40 it does
> solder through easily and does not char or burn. it just melts. Chemical
> strippers for UV40 have to be viewed with a lot of caution as they are
> highly aggressive to everything around it. Also, you have to ensure you
> remove it all or confirm the residues are harmless (very unlikely).
>
> Best Regards
>
> Lee Hitchens
> Technical Director
> SCH Technologies is a Division of SCH Services Limited
> Mob: +44 (0) 7862 25 33 21 www.conformalcoating.co.uk
>
> The opinions expressed in this e-mail are strictly those of the sender and not of SCH Services Limited. This communication may contain information which is confidential and may also be privileged. It is for the exclusive use of the intended recipient(s). Unauthorised use, copying or disclosure of any of it may be unlawful. If you are not the intended recipient(s) please note that any distribution, copying or use of this communication or the information in it is strictly prohibited. If you have received this communication in error please notify us by e-mail or by telephone (+44 (0)1226 249019) and then delete the e-mail and any copies of it. Virus Warning - Although steps have been taken to ensure that all email and attachments are virus-free, we cannot guarantee nor be held liable.
>
> Company Registration: 04043334
> Registered office: SCH Services Limited Newburgh Building McLintock Way Barnsley South Yorkshire S70 6BF
>
>
> On 29/05/2013 18:57, Richard Kraszewski wrote:
>> Those of you who have done or have tried doing this realize what type of challenge this can be. Thought I had resolved this some years ago, but now with the obsolescence of some strippers and increase in the various UV coatings we apply, I need to address this again. I can readily see that some UV coatings are much easier to strip that others.
>>
>> What type of chemical strippers do you guys use (both local & full)?
>>
>> Thanks
>>
>> Rich Kraszewski /PLEXUS
>>
>>
>> ______________________________________________________________________
>> This email has been scanned by the Symantec Email Security.cloud service.
>> For more information please contact helpdesk at x2960 or [log in to unmask]
>> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|