TECHNET Archives

April 1997

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wGrw6-000Bj2C; Mon, 14 Apr 97 15:01 CDT
Content-Type:
text/plain; charset=US-ASCII
Old-Return-Path:
Date:
Mon, 14 Apr 97 15:10:32 -0500
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
Content-Transfer-Encoding:
7bit
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/11937
From [log in to unmask] Mon Apr 14 16:
04:26 1997
TO:
Return-Path:
<TechNet-request>
X-Status:
Resent-Message-ID:
<"zkwur2.0.MfE.5qeKp"@ipc>
Subject:
From:
"Ron Hollandsworth"<[log in to unmask]>
X-Loop:
Mime-Version:
1.0
X-Mailer:
ccMail Link to SMTP R6.00.01
Message-Id:
Parts/Attachments:
text/plain (23 lines)

     Has anyone out there performed some hot and cold slump test?  Have you 
     run accelerated hot slump tests on paste?  If so at what temperatures?
     
     Is there a test plan for these tests?  If so, where can I find the 
     documents to follow the test plan?
     
     Thanks
     [log in to unmask]


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2