Rob,
Mil-STD-2000 is cancelled without replacement. Most people are going to
J-STD-001 and IPC-A-610, class 3 as a replacement.
Eric Kalgren
Manufacturing Engineer
Atlantic Microwave
Phone: 978-779-7062
Fax: 978-779-0101
-----Original Message-----
From: Robert Coburn [mailto:[log in to unmask]]
Sent: Monday, November 29, 2004 8:53 AM
To: [log in to unmask]
Subject: [TN] Standard status
Morning T'neters;
I'm trying to identify the status of MIL-STD-2000.
If it has been superseded, what is the doc #?
Is there an equivalent IPC doc?
TIA,
Rob
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|