In a message dated 02/02/2000 11:15:20 AM Central Standard Time,
[log in to unmask] writes:
<< I have my own thoughts of likes and dislikes on this issue but I would like
to know what everyone else thinks about Scoring Vs break away tabs.
Scott Lefebvre
530-265-1041
[log in to unmask] <mailto:[log in to unmask]>>>
Hi Scott!
My preference is v-scoring (with the comment that it has to be done properly
and the correct depth specified for the laminate type and thickness). Nothing
worse than having a panel fall apart on you half-way through the build, or
not being able to singulate each board after building it without a bunch of
force.
The reasons I like scoring is that theres a nice clean edge left on the
boards without the little "nubs" from the "rat-bites" (or the drilled holes
for the perforations of the tabs). Another thing that scoring eliminates, is
that with tabs I've experienced a lot of board damage from people not making
sure they've fractured all the glass fibers by bending in both directions
when breaking away the coupon of a panel. They bend in one direction and the
try to pull the coupon away and wind-up taking a little strip of laminate
with it at the tab area...sometimes ripping up a trace or two. I've never had
that happen with a scored panel.
-Steve Gregory-
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|