Has anyone used the company called Onyx to have their Lamination rolls coated?

Has anyone ever used the new chemical resistant Lamination rolls and has there been any changes in the quality of film adhesion? Has anyone noticed that the rolls last longer or a problem with durometer of the rolls changing faster?

***************************************************************************