Vesication??
Brian
Ken Bloomquist wrote:
> Happy Monday All,
>
> This has nothing to do with the ISS or Lawrence Welk :-)
>
> On occasion we get tiny bubbles in our moisture cure, polyurethane conformal
> coating. We know that if the humidity is high (seldom happens here in
> Western Washington) and you get the coating on a little thick the bubbles
> will form. I'm sure the coating skins over really fast in high humidity and
> then all those little volatiles can't get out creating tiny bubbles.
>
> My question is, are there any methods for removing these little bubbles once
> the coating is cured? Generally they are not bad enough to need rework but
> on occasion there are just too many to ignore.
>
> Thanks as usual for any help,
>
> KennyB
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|