TECHNET Archives

January 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Russell Burdick <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Russell Burdick <[log in to unmask]>
Date:
Mon, 17 Jan 2005 07:31:04 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (28 lines)
Good Morning Technetters,

I have a customer who is questioning the surface look of immersion silver
boards. They had assembled some and halted due to the look of a dark/black
tarnish on the silver finish.

The boards were made and the silver finish applied in China then sent to
subcontractor to assemble. The 3 boards in my gloved hands have one side
with no tarnish or surface irregularities and the second side on has the
dark/black tarnish look on surface pads and a few knees of holes appear
reddish (using a 10X lupe).

What can anyone offer for advice on solderability issues?

Thanks in advance,

Russ Burdick

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2