TECHNET Archives

October 1997

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Fulton Feng <[log in to unmask]>
Date:
Wed, 15 Oct 1997 16:59:13 -0400
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Fulton Feng <[log in to unmask]>
Parts/Attachments:
text/plain (93 lines)
Blachet
You can do one more thing that is to wash the boards you suspect
soldering problem in wave before going through wave soldering. In your
case, you said they could be solderd manually after washed, this telling
me some contamination issue, either grease or something else. If this
does not work out, probably you need to look at the orientation of the
wave flow. Good luck!



>----------
>From:  Blanchet,Richard[SMTP:[log in to unmask]]
>Sent:  Wednesday, October 15, 1997 9:01 AM
>To:    [log in to unmask]
>Subject:       [TECHNET] FW: [TECHNET] Assy: Soldering on gold plated pads
>
>Sorry if my previous note didn't contain all the info.
>
>I have problems with SOIC 16 tom and SOIC 14 and also with small 0805, 1206
>resistors.
>I'm running at 4.0 ft/min.
>I cannot change the rotation of the board because of the solder theives that
>have been designed to help me. By the way, sometimes the solder theives are
>not soldered. This is not a defect but and indication that something is
>wrong.
>The pads have been designed for wave soldering as far as I know. It's just
>that I get more of this problem near the fingers. Detachable rails would
>surely help but they wouldn't resolve the problem 100% since the problem is
>found elsewhere.
>
>Thank you.
>
> ----------
>From: owner-technet
>To: TechNet
>Subject: Re: [TECHNET] Assy: Soldering on gold plated pads
>Date: 15 October, 1997 10:14
>
>Charles Barker@IO-US
>10/15/97 10:14 AM
>
>Mr. Blanchet:
>
>What kind of components are you having problems with? SOT-23, passive
>chips, I. C.'s? Were the pads on this side of the board designed with wave
>soldering in mind?
>
>Can you rotate the board and send it through the wave in a different
>direction?
>
>What is your conveyor speed?
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe:   SUBSCRIBE TECHNET <your full name>
>To unsubscribe:   SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
>847-509-9700 ext.311
>##############################################################
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe:   SUBSCRIBE TECHNET <your full name>
>To unsubscribe:   SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
>847-509-9700 ext.311
>##############################################################
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2