could be the decap damage... if it is not cavity type part... (even it is
cavity type part, some sloppy decap job still can damage it...), at this
stage, you most likely have no case - dumpster diving is un-likely for TI
part... Look like analog amp stuff, could be wrong... (12 V? might be).
jk
> I understand this as a possibility, but I am used to seeing the scratches
> having what looks like shattered glass at the edge of the indentation. And
> I've never seen the segmented kind of features. And usually you can see a
> lot of differences in the focus plane.
>
> But yes, I agree that the parentage of this part needs to be certified!
>
> Wayn
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo
> Sent: Friday, October 09, 2015 2:45 PM
> To: [log in to unmask]
> Subject: Re: [TN] Ropy grunge in IC
>
> yap, like P-doped glass passivation scratch to me. (zig zag no
> crystallography fracture, so it is not die cracking... ;-).
> jk
>> I'm an old semiconductor reliability engineer (and this die looks like
>> it's old technology too :) ) - that looks like a scratch on the die.
>> So either it was untested by the manufacturer or it was scrap acquired
>> by dumpster diving (or some other nefarious method), packaged and sold
>> as a functional device...i.e. counterfeit.
>>
>> Mike
>>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|