We've used two materials (assuming you want white ink, other colors
available from vendors).
Cat-L-Ink 50-100 (resin) and #9 Catalyst Hysol
Division, Dexter Corporation, City of Industry, CA
ER-112 (resin)/ER-176 (catalyst), Naz-Dar Co., Chicago,
IL
> ----------
> From: Tomer_2[SMTP:[log in to unmask]]
> Sent: Sunday, October 12, 1997 5:43 AM
> To: [log in to unmask]
> Subject: [TECHNET] Legend ink
>
> Hi everybody
>
> I would like to hear from anyone who apply legend before HAL, since
>
> I need a white marking ink with the following properties:
>
> 1. No yellowing ( or other change in colour)even after several
> temperature process, and specally after HAL.
>
> 2. Good adhesion on conventional solder resist as well as metal.
>
> 3. Should be cured thermally
>
> I am looking for supplier name with the above ink.
>
> Any information on this would be much appreciated
>
> Tomer
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV
> 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> 847-509-9700 ext.311
> ##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|