TECHNET Archives

August 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
James Verrette <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, James Verrette <[log in to unmask]>
Date:
Wed, 9 Aug 2006 20:05:36 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (40 lines)
It is FR-4 in molded polycarbonate housing.

________________________________

From: [log in to unmask] [mailto:[log in to unmask]] 
Sent: Wednesday, August 09, 2006 7:44 PM
To: James Verrette; [log in to unmask]
Subject: Re: [TN] Routed edge tolerance


Hi Jim,
I do not know what kind of housing you are putting your PCB in, but from
your outline description I am guessing some cast housing. You are also
not giving us a clue about your application. You are also talking about
punching instead of routing, so i am guessing CEM-3 instead of FR-4 as
the PCB material.
In that case, your routing tolerances are your least problem; much more
worrisome are likely the different thermal expansions of the PCB and the
housing as well as swelling of the CEM-3 with moisture absorption.
GM ran into this with their windshield wiper controls: single-sided
CEM-3 PCBs in some combination of routing and housing tolerances
requiring press-fitting the PCBs. The result: windshield wiper failures
for some of the more high-end [read: high-powered=running hotter] SUVs
within as little as 1 year after sale due to solder joint failures
caused by PCB warping-over 4 million vehicles were ordered by NHSTA to
be recalled. 

Werner


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2