TECHNET Archives

December 2016

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Lehmicke, Michael" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Lehmicke, Michael
Date:
Wed, 14 Dec 2016 20:38:44 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (85 lines)
Victor;

I was thinking of multiple sample head. I am familiar with some Auto grinders that will hold 4 and 6 samples at once. I was wondering if any of the equipment on the market can grind more than 6 at the same time.

Mike Lehmicke
Project Engineer
DSS Division
Molex, LLC-Printed Circuit Solutions
22 Empire Drive
St. Paul, MN 55103
651-846-7728
[log in to unmask]



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: Wednesday, December 14, 2016 8:59 AM
To: [log in to unmask]
Subject: Re: [TN] Grinders/polishers for x-sections

-- Sent by an external Sender --

Single or multiple sample head AUTO GRINDER/POLISHER?

Victor,

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Louis Hart
Sent: Wednesday, December 14, 2016 7:54 AM
To: [log in to unmask]
Subject: Re: [TN] Grinders/polishers for x-sections

Mike, I was thinking of asking a similar question myself. I saw the responses of Vladimir and Dave a few minutes ago.

Buehler equipment has held up well here, which lasting 15 and more years, and in one case only failing after about 30 years as a result of an 'environmental mishap'.  Decades ago I worked at the Duke Engineering School's Materials Science department. There and ever since, I've heard encomiums of praise for Stuers but the initial costs seem to be 50% or more greater than competitors.

Struers has one or two 'demonstration vans' outfitted with all manner of sample preparation and inspection equipment. It or they spend the winter months in the south, if my understanding is correct. The one I saw was a surprise: a huge, luxury 'motor home', seeming to be, inside and out, made of some kind of stainless steel with customized equipment installations and as clean as you would want your hospital to be.  Louis Hart -----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lehmicke, Michael
Sent: Wednesday, December 14, 2016 12:52 AM
To: [log in to unmask]
Subject: [TN] Grinders/polishers for x-sections

This may generate a lively discussion.

What is the best Auto Grinding/Polishing system for high volumes of x-sections?

Thanks,

Mike

Mike Lehmicke
Project Engineer
DSS Division
Molex, LLC-Printed Circuit Solutions
22 Empire Drive
St. Paul, MN 55103
651-846-7728
[log in to unmask]<mailto:[log in to unmask]>

[cid:[log in to unmask]][cid:[log in to unmask]]<http://www.molex.com/>


________________________________



CONFIDENTIALITY NOTICE: This message (including any attachments) may contain Molex confidential information, protected by law. If this message is confidential, forwarding it to individuals, other than those with a need to know, without the permission of the sender, is prohibited.

This message is also intended for a specific individual. If you are not the intended recipient, you should delete this message and are hereby notified that any disclosure, copying, or distribution of this message or taking of any action based upon it, is strictly prohibited.

English | Chinese | Japanese
www.molex.com/confidentiality.html

________________________________



CONFIDENTIALITY NOTICE: This message (including any attachments) may contain Molex confidential information, protected by law. If this message is confidential, forwarding it to individuals, other than those with a need to know, without the permission of the sender, is prohibited.

This message is also intended for a specific individual. If you are not the intended recipient, you should delete this message and are hereby notified that any disclosure, copying, or distribution of this message or taking of any action based upon it, is strictly prohibited.

English | Chinese | Japanese
www.molex.com/confidentiality.html

ATOM RSS1 RSS2