TECHNET Archives

February 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Marcello Brett Malteze <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Marcello Brett Malteze <[log in to unmask]>
Date:
Fri, 24 Feb 2006 17:40:39 -0300
Content-Type:
text/plain
Parts/Attachments:
text/plain (61 lines)
Hey Team,


 


 


    We are facing some problems regarding voids on Via in Pad on a 10 layers


board with sequential lamination ( 3 times inside press) on BGA area ,


someone can give me light or share your experience on this?


 


Board Spec:


 


Dielectric 2 x 106 = 90 - 100 µm final


YAG machine


O/L Copper 12 µm


Laser Diameter 130 µm


Surface finish Immersion Tin


 


Sometimes Voids are so big that are creating shorts under BGA.


 


Marcello Brett Malteze 


Mechanical Process Engineering 


Mobile: + 55 11 9468 4833 


Skype: mbrett73 








Legal Disclaimer:

The information contained in this message may be privileged and confidential. It is intended to be read only by the individual or entity to whom it is addressed or by their designee. If the reader of this message is not the intended recipient, you are on notice that any distribution of this message, in any form, is strictly prohibited. If you have received this message in error, please immediately notify the sender and delete or destroy any copy of this message



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2